Scratch Damage In Ceramics: Role Of Microstructure

Scratch tests were conducted using a standard pyramid indenter against a-SiAION ceramics with different microstructures: (i) fine equiaxed grains and (ii) large elongated grains.

Author
Z Xie Et Al
Origin
University Of N S Wales, Australia
Journal Title
J Am Ceram Soc 86 1 2003 141-148