Schott Introduces Lead-Free Glass

Schott North America Inc. has introduced lead- and arsenic-free P-SF67 glass with a refractive index of 1.90680, a glass transformation temperature of 493 °C and an Abbe number of 21.40. The glass is suitable for the production of aspherical lenses used in compact lens systems. Aspherical lenses fashioned from this glass reduce the size and weight of camera phones, digital cameras, sports optics and medical devices. The company says that a single aspherical lens can compensate for image distortion and spherical aberration as efficiently as several spherical lenses can. The P-SF67 glass is available as polished preforms.

Author
Un-named
Origin
Unknown
Journal Title
www.Photonics.com/Article.Aspx?Aid=27326
Sector
Domestic glass
Class
D 1186

Request article (free for British Glass members)

Schott Introduces Lead-Free Glass
www.Photonics.com/Article.Aspx?Aid=27326
D 1186
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.