Saxs Study Of The Micro-Inhomogeneity Of Industrial Soda-Lime-Silica Glass

The microstructure of a variety of industrial multicomponent soda-lime glasses for containers and glazing and of a lead silicate glass for pressed tableware articles was analysed using small angle X-ray scattering (SAXA). No inhomogeneity with size .0,5nm was found in the industrial samples, while ternary soda-lime glass samples with suitable composition developed under heat treatment a phase separation easily detected by SAXS. The results obtained disprove earlier reports which attributed problems of rheology and strength affecting container production ("poor workability") to microstructure formations.

Author
A Benedetti Et Al
Origin
Unknown
Journal Title
Rivista Staz Sper Vetro 25 5 1995 179-188
Sector
Domestic glass
Class
D 237

Request article (free for British Glass members)

Saxs Study Of The Micro-Inhomogeneity Of Industrial Soda-Lime-Silica Glass
Rivista Staz Sper Vetro 25 5 1995 179-188
D 237
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
12 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.