Saint-Gobain Sekurit Invests For Future Of Motoring

Saint-Gobain has announced a EUR 4 million investment for its Sekurit autoglass plant at Avilés (Asturias, northern Spain). The aim is to upgrade plant machinery in order to meet the challenge of complex, sophisticated products that will be demanded of the motor industry in the future, said Ricardo de Ramón, director general of Saint-Gobain Sekurit for Spain and Portugal. The Avilés plant currently produces around 2.2 million, high-value windscreens per annum, making it the Sekurit group's leading plant in Europe.

Author
Un-named
Origin
Unknown
Journal Title
Glassonline News 11/02/05
Sector
News Items
Class
N 1672

Request article (free for British Glass members)

Saint-Gobain Sekurit Invests For Future Of Motoring
Glassonline News 11/02/05
N 1672
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 11 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.