Saint-Gobain Building Glass Introduces Its Best Performing Conservatory Roof Glass

Saint-Gobain Building Glass has further enhanced its popular collection of conservatory roof glass, with the introduction of Azura+ (launched April 2017) setting new benchmarks for the lowest g-value in the SGG BIOCLEAN low maintenance self-cleaning range. More than a year’s development has gone into incorporating the best solar performing low maintenance self-cleaning coating onto the popular Sapphire Blue tinted substrate, offering an 83% heat reflection and 0.17 g-value, firmly placing the product at the top of Saint-Gobain’s roof glass range.

Author
Un-named
Origin
Unknown
Journal Title
Https://www.Glassonweb.com/News/Saint-Gobain-Launches-Azura
Sector
Flat glass
Class
F 3965

Request article (free for British Glass members)

Saint-Gobain Building Glass Introduces Its Best Performing Conservatory Roof Glass
Https://www.Glassonweb.com/News/Saint-Gobain-Launches-Azura
F 3965
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
13 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.