Safety Testing Of Agglomerated Corks Used As Closures For Sparkling Wine Bottles (Italian)

A ten month trial to compare agglomerated and conventional cork closures showed that the agglomerated corks had better barrier properties. Tabulated results indicated the variation in internal pressure inside the bottles over the test period and the force required to open the bottles.

Author
L Lodovichi, F Chiti
Origin
Unknown
Journal Title
Ind Bevande 1988 17 93 32-39
Sector
Container glass
Class
C 77

Request article (free for British Glass members)

Safety Testing Of Agglomerated Corks Used As Closures For Sparkling Wine Bottles (Italian)
Ind Bevande 1988 17 93 32-39
C 77