[Russia] Magnezit Pushes On With Refractory Overhaul

Magnezit announced recently that it had widened its range of refractory products by adding new grades of bricks for the glass making industry. The first batch of bricks were manufactured at the Satka (Chelyabinsk) production site in July and have already been shipped. These are MZ-84 grade, made specifically for lining walls and regenerator checkers of glass-melting furnaces.

Author
Un-named
Origin
Unknown
Journal Title
Industrial Minerals August 2014 21
Sector
Refractories
Class
R 811

Request article (free for British Glass members)