[Russia] Balakhnistokoye Glass Signs Equipment Deal

The Nizhny Novgorod branch of Globus Leasing, participating in a large-scale investment project in the Russia's Volga-Vyatka region, has leased equipment for the production of silk screen decorated bottles to Balakhninskoye Glass (Balakhninskoye Steklo). The project investments were RUR 60M, including RUR 35M for the purchase of the equipment, the company said.