The "Rpr" Process For Repairing Silica Lining In Glass Furnaces

FIB's "RPR" (Reactive Projection for Repair) system produces thick and dense silica based coatings for repairing degraded silica parts of glass furnace superstructure. The choice of composition insures a strong bonding between the old masonry and the repair material whose properties are at least as good as those of the initial bricks. Comparision between several refractories shows that the material presents a high corrosion resistance and provides a real improvement of glass furnace life duration.

Author
O Diloreto Et Al
Origin
Fib Services, Belgium
Journal Title
Int Glass Journal 91 Jan/March 1997 60-62
Sector
Refractories
Class
R 215

Request article (free for British Glass members)

The "Rpr" Process For Repairing Silica Lining In Glass Furnaces
Int Glass Journal 91 Jan/March 1997 60-62
R 215
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 9 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.