The Role Of Surface And Volume Defects In The Fracture Of Glass Under Quasi-Static And Dynamic Loadings

In this paper, the role of surface & volume defects on fracture in soda-lime glass is analysed when samples are submitted to quasi-static or dynamic loadings. To investigate fracture, different experiments are carried out: quasi-static compression of glass spheres & edge-on-impacts. The first test series aims at studying crack initiation. Different surface treatments are performed to study their influence on the failure load, from which it is concluded that initiation of cracks occurs in the vicinity of the contact surface. The second series is concerned with the examination of crack patterns under dynamic loadings with two different strikers. Crack initiation under dynamic load histories is investigated near & far from the impact zone and it is concluded that it cannot take place within the volume, except in a very small zone close to the impact point.

Author
X Brajer Et Al
Origin
Saint-Gobain Recherche, France
Journal Title
J Non-Cryst Solids 316 2003 42-53
Sector
Special Glass
Class
S 2864

Request article (free for British Glass members)

The Role Of Surface And Volume Defects In The Fracture Of Glass Under Quasi-Static And Dynamic Loadings
J Non-Cryst Solids 316 2003 42-53
S 2864
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
18 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.