The Role Of Design And Refractory Specification On Furnace Campaign Life

This article reviews the influence of glass furnace design parameters and their effect on campaign life, with particular reference to the specification of refractory materials. Most of the information discussed concerns fuel-fired soda-lime glass furnaces, with mention of other compositions.