The Role Of Coatings And Other Surface Treatments In The Strength Of Glass

This report provides an introduction to the role of coatings and other surface treatments in the strength of glass. Sectors covered are: glass containers; flat glass, and glass fibre. The report is divided into the following parts: A quick review of generic approaches; what works and why? hot end/cold end coatings on containers; coatings on glass fibers; water/corrosion versus mechanical damage; tools for the evaluation of coatings; and, a summary.

Author
C G Pantano
Origin
Pennsylvania State University, Usa
Journal Title
www.Gmic.org/Strength%20In%20Glass/Pantano%20Pac%20Rim.Pdf
Sector
Special Glass
Class
S 3756

Request article (free for British Glass members)

The Role Of Coatings And Other Surface Treatments In The Strength Of Glass
www.Gmic.org/Strength%20In%20Glass/Pantano%20Pac%20Rim.Pdf
S 3756
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.