Role Of Al Formers And Na Modifiers In Al203-Si02-Na20-Mg0-Eu203 Glasses: Brillouin And Raman Spectroscopy Studies

Brillouin and Raman spectroscopies were used to investigate the structure of xAl203.(72.08-x) Si02.14.81Na20.11.85Mg0.1.26Eu203 (x=O, 2.96, 5.92, 8.88, 14.81 mol%) and yNa20. (83.93-y) SiO2.2.96Al203.11.85MgO.1.26Eu2O3 (y=9.86, 14.81, 19.73, 24.67 mol%) glasses. The depolymerisation of the Eu3+ doped soda magnesia aluminosilicate (EDSMAS) glass is mainly characterised by the presence of nonbridging (bridging) oxygens and three (four) member silicate and aluminosilicate rings. The aluminium formers entering the glass recover Si-O-Si bridges by attracting charge balancing modifiers from depolymerized SiO4 network. In this way the (Si,Al)4 rather than (SiAl)3 membered rings are formed, i.e. the overall structure becomes more polymerised rather than fragmented. This is supported by the glass elastic constants and moduli as measured by Brillouin spectroscopy.

Author
Z N Utegulov Et Al
Origin
Oklahoma State University, Usa
Journal Title
Phys Chem Glasses 45 3 2004 166-172
Sector
Special Glass
Class
S 2809

Request article (free for British Glass members)

Role Of Al Formers And Na Modifiers In Al203-Si02-Na20-Mg0-Eu203 Glasses: Brillouin And Raman Spectroscopy Studies
Phys Chem Glasses 45 3 2004 166-172
S 2809
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.