Rockware Claims Two-Pint Milk Bottle First

Rockware Glass has developed the two-pintie in conjunction with Associated Fresh Foods, Leeds, dairy. The bottle weighs 517g and its height is 265mm. It features a moulded grip. It is currently being test marketed and is available by doorstep delivery only.