The Ris Machine - A Performance Report

Experience with the Rotary Individual Section machine is reported. After initial difficulties an average percentage pack of 90.93% was achieved for the first nine months of 1989.

Author
H J Moder
Origin
Oberland Glas Ag
Journal Title
Glass International December 1989 31, 33