Rheological Properties And Isochomal Workability Of Lead Silicate Glass Melts

Four different industrial lead silicate glass melts were investigated by means of the cylinder compression method with respect to the flow and stress generation behaviour, the critical deformation rate, and the high-temperature tensile strength.

Author
Y Yue & R Bruckner
Origin
Technische Universitat Berlin, Germany
Journal Title
Glastech Ber Glass Sci Technol 69 9 1996 278-284
Sector
Special Glass
Class
S 1087