Rexam Invests At Dongen

Rexam Glass has invested more than Euros 15M in its factory near Dongen in the Netherlands. The furnace has been improved to cut energy consumption and NOx emissions and to melt batch with a higher proportion of cullet. The cold end has a renewed layout with a new concrete floor, automated palletisers and carriers; reject glass conveyors moved below the floor and covered transport lines and packaging equipment.

Author
Un-named
Origin
Unknown
Journal Title
Glass July 2004 143
Sector
Container glass
Class
C 2371

Request article (free for British Glass members)

Rexam Invests At Dongen
Glass July 2004 143
C 2371