Review On Enamel Equipment Repairing (In Chinese)

The peeling of enamel equipment was analysed in this paper. The authors describe the development of enamel equipment repairing around the world.

Author
Un-named
Origin
Unknown
Journal Title
Glass & Enamel 27 4 August 1999 57-60