Resonance Effects In Photoluminescence From Deep Traps In Cdsxse(1-X) Doped Glasses

Photoluminescence studies on CdSxSe(1-x) semiconductor doped glasses with gap energies ranging from 2 to 3 eV (400-600nm) are presented.