Researchers Find Recycled Glass Is Cheaper Way To Filter Raw Water

The use of recycled glass to put back into the glass production process is well-documented, but researchers in Singapore have now discovered a new application, which involves taking waste glass ceramic membranes to filter raw water, as this report explains.

Author
W Wong
Origin
www.Channelnewsaisa.com
Journal Title
Glass International Feb/12 25
Sector
Container glass
Class
C 4636

Request article (free for British Glass members)

Researchers Find Recycled Glass Is Cheaper Way To Filter Raw Water
Glass International Feb/12 25
C 4636