Research On Properties Of Rock-Mineral Wool As Thermal Insulation Material For Construction

Rock wool and slag wool pertain to the same kind of thermal insulation material, which can be produced in quantity and widely used, by comparison with other inorganic fiber thermal insulation materials, thus it is one of the most important thermal insulation material for the national economic development in our country. After the implementation of Civil Construction Energy Efficiency Management Regulation, it puts forward higher requirements for the energy saving standard of new buildings, thus the application prospect of rock-mineral wool thermal insulation material is promising. This paper mainly presents the source of rock-mineral wool, its main relative merits as well as its application in the construction field, moreover, the application and development potential of rock-mineral wool as the thermal insulation material for building wall construction.

Author
J Zheng Et Al
Origin
Unknown
Journal Title
Advanced Materials Research 450-451 2012 618-622 www.Scientific.Net/Amr.450-451.618
Sector
Glass Fibre
Class
GF 703

Request article (free for British Glass members)

Research On Properties Of Rock-Mineral Wool As Thermal Insulation Material For Construction
Advanced Materials Research 450-451 2012 618-622 www.Scientific.Net/Amr.450-451.618
GF 703
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 12 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.