Reproducibility Of The Structure And Properties Of Parts And Their Description Within The Framework Of Nonlinear Dynamics

The problem of the reproducibility of complex structures is discussed from the standpoint of the applied theory of dynamic systems. Some fundamental concepts of the theory of nonlinear fluctuations (bifurations, fractal sets, space and time networks of interacting subsystems) that can be helpful in applications are described on a quantative level.

Author
A Yu Loskutov
Origin
Moscow State University, Russia
Journal Title
Glass And Ceramics 57 7-8 2000 243 - 247
Sector
Special Glass
Class
S 3171

Request article (free for British Glass members)

Reproducibility Of The Structure And Properties Of Parts And Their Description Within The Framework Of Nonlinear Dynamics
Glass And Ceramics 57 7-8 2000 243 - 247
S 3171
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.