Castolin Eutectic recently launched its comprehensive new range of low temperature nickel-based Eutalloy spray/fuse powders which are specifically designed to work with the repair and manufacture of glass container moulds. In this article, the author reviews recent developments in the methods and materials used to protect and repair glass container moulds.