Removing Ferrous And Non-Ferrous Components

Magnets eliminate metal contamination, helping prepare cullet for re-melting in the glass furnace. Recycled glass can only be processed once all traces of metal have been removed. Separating and recovering ferrous and non-ferrous metal is now quite simple, even under the most demanding circumstances, thanks to the latest magnetic materials used in Goudsmit Magnetic Systems equipment, as described in this article.

Author
P Ector
Origin
Goudsmit Magnetic Systems, Netherlands
Journal Title
Glass July-August 2007 23