Remaining Structural Capacity Of Broken Laminated Safety Glass

To confirm the load carrying capacity of overhead glazing, accessible glass and all other basic glass sections, modern calculation procedures are used and a verification of the remaining structural capacity is required. This verification is typically done by full scale tests. This project is part of the EU COST action C13 Glass & Interactive Building and aims at formulating mechanical models to describe load transfer mechanisms in broken glass in order to satisfy safety requirements.

Author
Un-named
Origin
Unknown
Journal Title
Proc Glass Processing Days, Tampere, 2004 403-407
Sector
Flat glass
Class
F 1542

Request article (free for British Glass members)

Remaining Structural Capacity Of Broken Laminated Safety Glass
Proc Glass Processing Days, Tampere, 2004 403-407
F 1542
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
15 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.