Relaxation Of Ultrasonic Waves In Ternary Te02-V205-Sm203 Glasses

Studies were carried out on the attenuation of longitudinal ultrasonic waves in tellurite glasses containing vanadium and samarium oxides with different concentrations, using the pulse echo technique.

Author
M A Sidkey Et Al
Origin
National Inst For Standards, Egypt
Journal Title
Glastech Ber Glass Sci Technol 73 7 2000 199-203
Sector
Special Glass
Class
S 2002