Relationship Of Structual Phase Transformations And Properties Of Sol-Gel Films In The Bi2O3 - Tio2 - Fe2O3 System

It is shown that the structure and properties of gel-sol oxide films depend on the total mass content of film-forming oxides in the solution and are determined by the different degrees of nonequilibrium of the physiochemical processes. The existance of quite clear relationships between the solution viscosity, the specifics of the microstructure, and certain properties of the film is established.

Author
A B Atkarskaya Etal
Origin
Avtosteklo Production Company
Journal Title
Glass And Ceramics 57 3-4 2000 118 - 123
Sector
Special Glass
Class
S 3159

Request article (free for British Glass members)

Relationship Of Structual Phase Transformations And Properties Of Sol-Gel Films In The Bi2O3 - Tio2 - Fe2O3 System
Glass And Ceramics 57 3-4 2000 118 - 123
S 3159
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.