Relationship Between Crystallization And Shrinkage In Superfine Quartz Fibers And Their Impurities

Experiments to determine the crystallisation resistance and shrinkage of fibres in conditions of isothermal soaking are described. The relation to impurities in the composition of the glass fibre, the type of raw materials used originally and impurities in the composition of the rods used for drawing the fibres was also examined.

Author
M V Zasolotskaya Et Al
Origin
State Institute Of Research For Ceramics And Glass, Stekloplatik Npa
Journal Title
Glass And Ceramics 1988 45 1-2 23-26
Sector
Glass Fibre
Class
GF 51

Request article (free for British Glass members)

Relationship Between Crystallization And Shrinkage In Superfine Quartz Fibers And Their Impurities
Glass And Ceramics 1988 45 1-2 23-26
GF 51
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.