Refractory Minerals - Trends & Developments In Supply & Demand

Six refractory raw materials - bauxite, brown fused alumina, graphite, dead burned magnesia, refractory clays, and silicon carbide - are the focus of this paper. These materials are significant in that they represent some of the most important raw materials for the world refractories market, and are all sourced from China. This paper summarises the principal world and Chinese sources of these minerals, along with recent trends and developments that have influenced their supply and demand.

Author
M O'Driscoll
Origin
Unknown
Journal Title
Industrial Minerals 410 November 2001 33-34, 37, 39
Sector
Refractories
Class
R 413

Request article (free for British Glass members)

Refractory Minerals - Trends & Developments In Supply & Demand
Industrial Minerals 410 November 2001 33-34, 37, 39
R 413
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 16 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.