Refractory Contribution To Energy Savings In Glass Melting (In French)

Over the past two decades, energy consumption for one ton of glass has been reduced by approximately 25%. Refractories have strongly assisted this reduction. Other factors have also helped, such as the increase in recycled glass content, the changes in specific pull, furnace lifetimes, and the modification of furnace operating parameters with respect to environmental quality. For flame furnaces producing soda-lime glass, this article covers the changes in the recent decades in refractory solutions for every furnace zone, identifying the latest high-performance, innovative solutions which are currently accessible.

Author
J Roux
Origin
Sepr, France
Journal Title
Verre 7 6 Jan/2002 56-61
Sector
Refractories
Class
R 424

Request article (free for British Glass members)

Refractory Contribution To Energy Savings In Glass Melting (In French)
Verre 7 6 Jan/2002 56-61
R 424
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.