Refractories For Glass-Contact Applications (Spanish)

Refractories intended for glass-contact applications are reviewed. The use of high-purity raw materials and novel forming techniques in refractory manufacture is discussed.

Author
P Pena
Origin
Instituto De Ceramica Y Vidrio
Journal Title
Bol Esp Vidr 1989 28 2 89-96
Sector
Refractories
Class
R 28