Refraction And Density Of Barium Aluminium Flurophosphate Glasses

It has been shown that the atomic refraction, average refraction of oxygen and fluorine of glasses, the atomic volume and average fluorine of glasses, the atomic volume and average volume of oxygen and fluorine increase sharply with the addition of small amounts of Group II and III elements of the periodic system to flurophosphate glasses apart from those with AlF3