Reduction Of Lead Leaching From Crystal Glasses

The first part of this paper deals with surface treatment of crystal glass products by dealkalization at temperatures of 200-450 deg C. The second part is concerned with the results of a study aimed at suppressing the amounts of lead leached from lead crystal glasses by modifying their composition.

Author
M Rada
Origin
Unknown
Journal Title
Int Cryst Fed Tech Exchange Conf 1995 128-146
Sector
Domestic glass
Class
D 285

Request article (free for British Glass members)

Reduction Of Lead Leaching From Crystal Glasses
Int Cryst Fed Tech Exchange Conf 1995 128-146
D 285