Reduction In The Emission Of Nox From Glass Melting Furnaces

Quadraflo oxy-fuel burners have been successfully used at the Weiden plant of FX Nachtmann to reduce the emission of nitric oxides from glass-melting furnaces. This paper describes the background to this development and outlines the benefits.