Reducing Fishscale In Hot Water Tank Enamels

Fishscale is delayed chipping of the fired & cooled enamel finish. During firing, hydrogen enters the steel in the atomic form. Hydrogen is introduced into the steel from various sources, such as in the form of moisture in the furnace atmosphere, improperly dried bisque, water in clays, residue left during metal preparation, & products of combustion. During firing, the moisture reacts with the steel. As the temperature increases, solubility of atomic hydrogen (H) in steel increases to as much as 1000 times room temperature. As the enamel cools, the solubility of hydrogen decreases. Hydrogen that dissolved at the higher temperature now begins to diffuse & form molecular hydrogen (H2) at the steel/enamel interface. If pressure of hydrogen gas builds up enough to overcome the enamel adherence/strength of the enamel itself, then fishscale will occur.

Author
M Wilczynski & R Wallace
Origin
Unknown
Journal Title
Cesp 66 Porcelain Enamal Inst Tech Forum 25 5 2004 57-61
Sector
Enamels
Class
E 113

Request article (free for British Glass members)

Reducing Fishscale In Hot Water Tank Enamels
Cesp 66 Porcelain Enamal Inst Tech Forum 25 5 2004 57-61
E 113
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 15 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.