Reducing The Contamination Of Effluent Gas From Glass-Melting Furnaces

Experiments have been carried out to determine the effect of various methods of granulation on batch carryover in continuous glass furnaces. Three commercial furnaces melting 13, 10 and 14.5 tonnes/day respectively were used to melt flat, opal and borosilicate glasses with oil, natural gas and LPG as fuels. The results indicated that in all cases the use of granulated batches should enable significant reductions in atmospheric pollution to be achieved.

Author
I T Timofeeva Et Al
Origin
Unknown
Journal Title
Glass And Ceramics 44 1-2 January-February 1987 37-39
Sector
Special Glass
Class
S 5045

Request article (free for British Glass members)

Reducing The Contamination Of Effluent Gas From Glass-Melting Furnaces
Glass And Ceramics 44 1-2 January-February 1987 37-39
S 5045
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 11 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.