Redox Reactions During Cooling Of Glass Melts - A Theoretical Consideration

Kinetic effects during cooling have been investigated, starting from a thermodynamic description of redox equilibria in molten glass.

Author
C Russel
Origin
Universitat Erlangen-Nurnberg
Journal Title
Glastech Ber 1989 62 6 199-203
Sector
General
Class
G 256

Request article (free for British Glass members)

Redox Reactions During Cooling Of Glass Melts - A Theoretical Consideration
Glastech Ber 1989 62 6 199-203
G 256