Redox Equilibria And Constitution Of Polyvalent Ions In Oxide Melts And Glasses

It is shown that redox equilibria of polyvalent ions in glass melts cannot usually be considered without complex-formation reactions and therefore without ligand formation and coordination behaviour. Differences in behaviour at different temperature ranges are discussed.

Author
H Hirashima, T Yoshida, R Bruckner
Origin
Keio University, Technische Universitat Berlin
Journal Title
Glastech Ber 1988 61 10 283-292