Redox Conditions During The Melting Of Batch

During the melting down of glass batches a variety of gases are set free. The redox conditions of the melt can be influenced by these gases, because both the gases and the melt are at the same time in a temperature range of 200K. For the quantification of this influence batches with different charges of coal were heated in comparision with a batch without additions of coal. With the continuous measurement of the oxygen partial pressure and the content of CO in the gas the effect of coal on the reactions of gases during the heating of batches can be described.

Author
C Flick And G Nolle
Origin
Inst Fur Silikattechnik, Freiberg, Germany
Journal Title
Glastech Ber Glass Sci Technol 68 3 1995 81-83
Sector
General
Class
G 1230

Request article (free for British Glass members)

Redox Conditions During The Melting Of Batch
Glastech Ber Glass Sci Technol 68 3 1995 81-83
G 1230
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.