Redox Chemistry Of Iron-Manganese And Iron-Chromium Interactions In Soda-Lime-Silica Glass Melts

Glass melts are usually not in a chemical equilibrium with a coexisting gas phase, it does not adjust before maintaining the melt at a constant temperature and a constant gas phase for hours. However, the one-phase equilibrium between several polyvalent elements in a melt above the glass transition temperature always exists, it adjusts spontaneously. Below the transition temperature the redox state is invariably frozen-in. The calculation of redox states must be based on the matter and charge balance (stoichiometric equations) and equilibrium relations (mass-action law). Such a calculation of Schreiber's experimental results was consistently possible. Accordingly, cooled glasses are free from Cr6+ if the glass containes Fe2+. To achieve this one has to melt oxidized chromium-containing glasses with sufficient iron content.

Author
G Nolle
Origin
Freiberg, Germany
Journal Title
Glastech Ber Glass Sci Technol 71 1 1998 1-5
Sector
Special Glass
Class
S 1316

Request article (free for British Glass members)

Redox Chemistry Of Iron-Manganese And Iron-Chromium Interactions In Soda-Lime-Silica Glass Melts
Glastech Ber Glass Sci Technol 71 1 1998 1-5
S 1316
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.