Recycling Of Tv-Glass: Problems And Perspectives

In Germany there is an "Electronic Waste Order" in preparation and the electronic industry may be compelled to take back waste appliances and arrange for their disposal. Around 5m TV tubes are manufactured in Germany every year and new concepts to recycle these have to be found. In this paper, investigations in recycling TV glasses in a continous glass fibre process plant as a secondary raw material, where the hazardous components are bound in a glass matrix, are examined.

Author
S Cramer Et Al
Origin
Inst Fur Neue Materialien, Gmbh, Germany
Journal Title
Glastech Ber Glass Sci Technol 68 C2 1995 191-197
Sector
General
Class
G 1434

Request article (free for British Glass members)

Recycling Of Tv-Glass: Problems And Perspectives
Glastech Ber Glass Sci Technol 68 C2 1995 191-197
G 1434
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.