Recycling Special Glass (Cathode Ray Tubes)

When the container glass industry began using recycled cullet 20 years ago, it faced considerable difficulties. Since that time, the rate of recycling has been brought up to approximately 63% (in Germany 1993), with green glass having the highest rate at approximately 93%, while clear or brown glass account for only about 50%. The reasons for the limited rate of recycling in this case point to findings which can be directly applied to special glass. Schott has initiated a project to look for possiblities of utilisation ("new" products) and is also examining how to produce environmentally compatible materials by vitrifying contaminants while integrating recycled glass.

Author
H Tietze
Origin
Schott Glaswerke, Germany
Journal Title
Glastech Ber Glass Sci Technol 68 5 1995 165-170
Sector
Special Glass
Class
S 889

Request article (free for British Glass members)

Recycling Special Glass (Cathode Ray Tubes)
Glastech Ber Glass Sci Technol 68 5 1995 165-170
S 889
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
12 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.