Municipal solid waste incinerator (MSWI) ash and sewage sludge incinerator (SSI) ash represent a significant portion of the solid wastes generated by industrialised nations which must be ultimately re-used or landfilled. This paper discusses the recycling of incinerator ashes and other industrial solid wastes into high quality ceramic tile products via the use of a newly developed, fossil fuel fired, melting process integrated with an advanced tile manufacturing process. The patented technologies are based on an advanced in-flight suspension glass melting technology developed by Vortec Corporation of the US integrated with an advanced ceramic tile formulation and manufacturing technolgy developed by Welco Industriale of Italy.

Author
J G Hnat & C Peracino
Origin
Vortec Corp & Welko Ind Spa
Journal Title
International Glass Review Spring/Summer 1996 85, 87, 89, 91
Sector
Glass Ceramics
Class
GC 240

Request article (free for British Glass members)

Recycling Incinerator Ash Into High Quality Ceramic Tile
International Glass Review Spring/Summer 1996 85, 87, 89, 91
GC 240
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.