Recycling Of Electrostatic Precipitator Dust From Glass Furnaces

Electrostatic precipitators have found wide acceptance in the glass industry for abating particulate discharge from glass furnaces. In the past, relatively small amounts involved and the difficulties in handling the very fine, low-bulk-density material had made disposal in a landfill the least expensive method. Various efforts to improve the material handling characteristics, such as pelletization and roll compression, have had only mixed success. In this paper, the choice of equipment, modifications to complement the existing facility, material characteristics of the collected dust, and the process requirements for two systems are described.

Author
D T Boothe Et Al
Origin
D Boothe & Co Inc, Usa
Journal Title
Ceram Eng Sci Proc 15 2 1994 62-72
Sector
General
Class
G 1162

Request article (free for British Glass members)

Recycling Of Electrostatic Precipitator Dust From Glass Furnaces
Ceram Eng Sci Proc 15 2 1994 62-72
G 1162
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.