Recycling Electrostatic Precipitator Dust

The recycling of particulate discharge from the furnace back into the glassmaking process has come of age, believes D Boothe & Co. This paper describes two of the company's custom designed systems for handling the dust generated from electrostatic precipitators installed at the Niles (Ohio) and Lexington (Kentucky) plants of GE Lighting.

Author
D T Boothe
Origin
D Boothe & Co Inc, Usa
Journal Title
Glass International September 1994 73-74
Sector
General
Class
G 1149