Recent Progress In Solid State Nuclear Magnetic Resonance For The Structural Characterization Of Materials (In French)

the range of possible high resolution solid state nuclear magnetic resonance experiments for solids is subjected nowadays to a rapid evolution. this is linked both to the evolution of the hardware and to the description of new concepts in the excitation pulse sequences. This paper describes these new methods and their possible applications in the field of material sciences, inorganic or hybrid materials.

Author
Massiot D
Origin
Unknown
Journal Title
Spectra Analyse 21 Jan-Feb 2002 27-33
Sector
Special Glass
Class
S 2484

Request article (free for British Glass members)

Recent Progress In Solid State Nuclear Magnetic Resonance For The Structural Characterization Of Materials (In French)
Spectra Analyse 21 Jan-Feb 2002 27-33
S 2484
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.