Recent Advances In Heavy Metal Oxide Glass Research

The effects of silica additions to a heavy metal oxide base to derive compositions suitable for core and cladding of optical waveguides are described.

Author
J C Lapp, W H Dumbaugh, M L Powley
Origin
Corning Incorporated
Journal Title
Spie Vol 1327 Properties And Characteristics Of Optical Glass Ii 1990
Sector
Glass Fibre
Class
GF 68