Realistic Finite-Element Model For The Double-Torsion Loading Configuration

The analytical approach to the double-torsion, constant-displacement-configuration technique has forced a strong oversimplification of the specimen model, and, therefore, of the strain field in classical applications. For this study, accurate three-dimensional finite-element analysis was performed on a realistic specimen; that is, one with thickness, a groove, and an initial notch. The influence on the strain-energy release reate of the specimens width and length, fracture length, the presence and shape of the side groove, the presence of an initial notch, and the curved shape of the fracture front was estimated from this analysis. Significant deviations from the classical analytical solution were found.

Author
M Ciccotti
Origin
Univ Bologna, Italy
Journal Title
J Am Ceram Soc 83 11 2000 2737-2744
Sector
Special Glass
Class
S 2076

Request article (free for British Glass members)

Realistic Finite-Element Model For The Double-Torsion Loading Configuration
J Am Ceram Soc 83 11 2000 2737-2744
S 2076
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
12 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.