Reactive Molecular Dynamic Simulations Of Sodium Silicate Glasses - Toward An Improved Understanding Of The Structure

Reactive potentials are becoming increasingly popular as they are expected to bridge the gap between ab initio and classical molecular dynamics. However, their applicability and potential benefits to model multicomponent glass networks are yet to be assessed. Here, an archetypal modified silicate glass, sodium silicate glass, is simulated using the ReaxFF potential. The predicted structure is critically evaluated and compared to that obtained by a classical potential and experimental data. Results indicated that ReaxFF offers an improved description fo the atomic structure, both at the short and medium range. Particularly, owing to its bond order form that dynamically adjusts potential energies according to the local atomic environment, ReaxFF reproduces the effect of modifiers on the Si-O network, a demonstration of its good transferability to various compositions. Overall, ReaxFF provides a promising alternative to classical and ab initio methods for simulating complex structures and processes for multicomponent silicate glasses.

Author
Y Yu Et Al
Origin
University California, Usa
Journal Title
Appl Glass Sci 8 2017 276-284
Sector
Special Glass
Class
S 4408

Request article (free for British Glass members)

Reactive Molecular Dynamic Simulations Of Sodium Silicate Glasses - Toward An Improved Understanding Of The Structure
Appl Glass Sci 8 2017 276-284
S 4408
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 11 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.