Reactive Ion Etching (Cf4/Ar) And Ion Beam Etching Of Various Glasses For Diffractive Optical Element Fabrication

This paper reports on the reactive ion etching (RIE) and ion beam etching (IBE) of commercially available glasses and their usability for the fabrication of diffractive optical elements as an alternative for expensive quartz glass.